Update your NiMH battery pack knowledge COLUMN BY CRAIG VAN BATENBURG typical nickel metal hydride (NiMH) battery pack consists of as many 1.2 volt cells as needed to attain the high voltage required to run an elec- tric motor. Honda used 120 D cells that, when connected in series, produce 144 volts. Six cells were spot welded top to bottom and then covered in an orange plastic sheath. At each end a threaded nut was attached and a black heat sensitive flat sensor strip was trapped under the orange cover. Many of these “sticks” were then bolted into a black plastic case with orange ends. Toyota and many others use six NiHM cells (1.2 volts per cell) molded into one module that is square—not round. Then these modules are connected in series to attain the voltage specified, usually 200 volts or more. Eight cells per module have also been used. Once the case, in this instance made of metal, has the required cells, temperature sensors, a computer, a fan to keep it cool, and relays that connect the orange cables to the rest of the car, the battery pack is pretty much complete. How are they holding up? The big fear is that the expensive nickel metal hydride (NiMH) battery pack will fail after the warranty is up and all the fuel savings will not be realized. This rumor is wildly reported so that fear keeps some people away. Here is what I know; the high voltage (HV) battery pack in my 10-plus year old Insight is as good as new a A Honda NiMH cell being measured for voltage. with over 100,000 miles on it. A few NiMH cells have failed. Not many, but with over 2.6 million hybrids on the roads worldwide (Toyota hit 2 mil- lion in sales of hybrids in 2010), some- thing is bound to go wrong. Most NiMH battery packs that develop codes were swapped out under warranty. The Insight battery pack is a problem for some own- ers after 100,000 miles mostly due to a poorly designed regenerative braking sys- tem. (More about that in future articles.) Toyota has had a handful of warranty battery pack replacements that were not cell related, but corroded terminals within the pack on their Generation I (2001 to 2003) Prius. Honda had some Insights that sat too long and the cells degraded. They were warranted and now a warning label is under the hood. There is an extended war- ranty on early Insights for NiMH battery problems so check your information sources carefully before selling your cus- tomer a new high-voltage battery. As time goes on there will be battery replacements so make sure you are ready. Storage and safety If you are going to store a hybrid, here is what to do. Check the state of charge (SOC) of the big battery and if lower than 55 percent, run the engine or drive the car until it is at least that or higher. Sixty per- cent SOC is about normal. Then you can store the car for up to three months or longer without a problem. Remember Honda disagrees with my advice here. Heat is anegative factor but cold weather extends the time a hybrid can sit. Over that time period the NiMH (high-voltage) battery pack could start to lose its charge. If the NiMH drops below 20 percent SOC, it could cause some long-term battery life issues. SOC is measured with a scan tool. Honda hybrid cars will need to be An HYB hybrid battery tester. started and run for 30 minutes every three months in a hot climate. Honda says every 30 days. Toyota and Lexus have HV chargers but they are not available and pricy. So follow the Honda suggestion. ACDC has developed a technique we use in ACDC’s “Up Your Voltage!” class but it can be dangerous so we only offer this tip in hands- on class for safety and liability reasons. The 2005 to 2008 Ford Escape HEV (not sold outside the USA) HV battery can be charged in the car even if the engine will not start. Try this: Connect a battery charger to the 12 volt lead acid under the hood. Every month, switch the onboard HV charger switch on 2X. It is located on the left kick panel (2005 to 2007) and the left dash end panel (2008). It was elimi- nated on the 2009 and newer models and is not available on the Fusion HEV. The owner’s manual will offer more detailed instructions. The ability to recharge a low NiMH battery without special tools and equipment can be very useful. Here’s what to do BEFORE removing or touching HV parts (orange in color): ¢ Remove key and make sure car, not just the ICE, is off. If it is keyless (like the Toyota) make sure the dash is dark. ¢ Disconnect the 12 volt battery. ¢ Remove or switch “off” the main HV switch or plug. ¢ Test all HV parts with a CAT II DVOM while wearing your HV gloves. ¢ Don’t take chances. Work safely. Does the air conditioner work? In case you don’t already know, the air conditioning system either directly or indirectly cools the battery pack. Make sure the a/c is functioning well. This is good news for a/c shops as hybrids will be very good for business. Tools and equipment to consider One company stands out and that is Midtronics based in Chicago. Dan Cox attended ACD
File Type:
pdf
File Size:
2 MB
Categories:
eren